-
First quarter net income of $39.2 million or $0.74 per share.
-
First quarter net sales excluding raw material surcharge up 41% from a
year earlier on 36% higher volume.
-
Latrobe contributed $16.3 million of operating income in the first
quarter, and $0.07 per share accretion.
WYOMISSING, Pa.--(BUSINESS WIRE)--Oct. 23, 2012--
Carpenter Technology Corporation (NYSE:CRS) today reported net income
attributable to Carpenter of $39.2 million or $0.74 per share for the
quarter ended September 30, 2012. The net accretion from Latrobe’s
operating results offset by a higher share count, contributed $0.07 per
share.
“Our strong first quarter results demonstrate that we are continuing to
execute well against our strategic plan,” said William A. Wulfsohn,
President and Chief Executive Officer. “While there are some areas,
particularly in lower value products, where customer demand has softened
recently, our overall business continues to be well positioned in
attractive end markets with strong demand for our ultra-premium and
premium products. This is evident in our strong top line growth, and
continuing positive spread between our revenue and volume growth rates.
“Latrobe results, after seven months of ownership, remain strong and we
are still tracking ahead of our deal economics, with the acquisition
expected to be at least 10 percent accretive this fiscal year. The teams
are doing an outstanding job delivering operational synergies from the
combined operation that will lead to higher volumes, improved costs and
a richer mix. The first new VAR furnace recently began operation with
two more to come on-line in the near future. We are accelerating use of
the Latrobe assets for additional premium products, which will enable us
to continue improving mix and our average mill profit per pound.
“We also continue to identify opportunities, as part of the Latrobe
integration, to optimize asset utilization across the total mill
operation. There are several small, near-term consolidation
opportunities that we have begun to execute, and we continue to evaluate
other potential opportunities to optimize our system assets. In
addition, we have completed a study that identifies significant
inventory reduction opportunities across the mill system, which we will
begin to implement.
“We remain on track to achieve the financial targets we set for our full
fiscal year and expect strong 2nd half shipment levels. Strong customer
demand for the ultra-premium and premium parts of our product line,
combined with our large backlog is consuming our full available premium
capacity.”
First Quarter Results
Financial highlights for the first quarter of fiscal year 2013 include:
|
|
|
|
|
|
|
(in millions, except per share amounts
& pounds sold)
|
|
1Q
FY 2013
|
|
1Q
FY 2012
|
|
Net Sales
|
|
$544.9
|
|
$414.1
|
|
Net Sales Excluding Surcharge (a)
|
|
$440.8
|
|
$313.6
|
|
Operating Income Excluding Pension Earnings, Interest and Deferrals
(a)
|
|
$69.6
|
|
$47.6
|
|
Latrobe Transaction Costs
|
|
-
|
|
$1.4
|
|
Net Income Attributable to Carpenter
|
|
$39.2
|
|
$23.8
|
|
Diluted Earnings per Share
|
|
$0.74
|
|
$0.53
|
|
Net Pension Expense per Diluted Share (a)
|
|
($0.21)
|
|
($0.14)
|
|
Free Cash Flow (a)
|
|
($102.7)
|
|
($109.2)
|
|
Pounds Sold (000) (b)
|
|
64,014
|
|
47,028
|
(a) non-GAAP financial measure that is explained in the attached tables
(b) excludes pounds sold through distribution
Net sales for the first quarter were $544.9 million, up 32 percent from
the prior year. Excluding surcharge revenue, net sales were $440.8
million, up 41 percent from a year ago on 36 percent higher volume.
Excluding the Latrobe impact, first quarter revenue excluding surcharge
was up 9 percent on 4 percent higher volume.
Specialty Alloy Operations (SAO) segment sales without surcharge
increased 16 percent on 7 percent higher volume compared with the fiscal
year 2012 first quarter. Most of this growth occurred in the highest
value ultra-premium and premium products. SAO operating income was $54.4
million, with a 20 percent operating margin, on revenue excluding
surcharge. The Latrobe segment, which currently includes the Latrobe and
Mexico distribution businesses that are planned for divestiture,
contributed $15.7 million of operating income in the quarter, with a 15
percent operating margin. Latrobe continues to perform ahead of
announced deal economics due to strong progress on operational
synergies. Performance Engineered Products (PEP) segment sales increased
17 percent in the same period, essentially due to the inclusion of the
Specialty Steel Supply (SSS) energy distribution business. PEP operating
income was $11.5 million, with a 12 percent operating margin. Additional
segment information is available in the attached schedules.
Gross profit was $109.3 million compared with $81.1 million in the
fiscal year 2012 first quarter. The higher gross profit was driven by
the addition of Latrobe, and improvement in SAO due to increased volume
and a higher profit per pound from an improved product mix and higher
prices.
SG&A expense as a percentage of revenue excluding surcharge was 0.6
percent lower than the prior year first quarter. SG&A in the current
quarter was $47.7 million or 10.8 percent of revenue excluding
surcharge, compared with $35.7 million or 11.4 percent of revenue
excluding surcharge for the first quarter of fiscal year 2012. The
increase in spending primarily reflects the addition of Latrobe-related
overhead costs and higher pension expense.
Operating income for the first quarter was $61.6 million compared with
$44.0 million a year earlier. Excluding surcharge revenue and pension
earnings, interest and deferrals (EID), operating margin was 15.8
percent compared to 15.2 percent in the fiscal year 2012 first quarter.
Included in operating income were approximately $1.6 million, or $0.02
per share, of costs related to startup of the Athens, Alabama facility,
optimizing the Company’s manufacturing footprint post-Latrobe, and the
Company’s new inventory reduction initiative. In total, these costs
impacted overall operating margin by about 0.4 percent.
Interest expense in the quarter was $5.2 million compared to $7.0
million in the year-ago period when the debt level was temporarily
higher due to the timing of debt refinancing.
Other income was $2.7 million compared to other expense of $0.7 million
in the fiscal year 2012 first quarter, due almost entirely to positive
impacts in the funding mechanisms for certain non-qualified retirement
plans.
The provision for income tax was $19.6 million or 33.2 percent of
pre-tax income compared to $12.6 million or 34.7 percent of pre-tax
income in the first quarter of fiscal year 2012.
Net income attributable to Carpenter was $39.2 million or $0.74 per
diluted share. Net income attributable to Carpenter in the same quarter
a year ago was $23.8 million or $0.53 per diluted share.
Free cash flow, defined as cash from operations less capital
expenditures, dividends, and the net impact from the purchase and sale
of businesses, was negative $102.7 million in the current quarter
compared to negative free cash flow of $109.2 in the prior year first
quarter. Strong net income was offset by pension contributions, higher
capital spending and increased inventory levels. Much of the first
quarter inventory build reflects normal business seasonality and the
need to support strong balance of year business growth. Beyond this, the
Company has identified areas where it believes it can reduce inventory
and improve turns across the mill operations. Full year free cash flow
is still expected to be negative $125 million, due to $350 million in
expected capital spending, primarily for the Athens facility. The free
cash flow estimate currently excludes proceeds from the sale of the
distribution businesses, and anticipated improvements from the inventory
reduction initiative.
Markets:
Aerospace & Defense market sales were $252.6 million in the
first quarter, up 45 percent compared with the same period a year ago.
Excluding surcharge revenue, aerospace & defense sales were up 52
percent on 103 percent higher volume (or up 19 percent on 12 percent
higher volume without Latrobe). Aerospace growth continues to reflect
strong demand for Carpenter’s and Latrobe’s premium and ultra-premium
products. Increased demand for engine materials is being driven by the
higher build rate of larger engines and share gain. Demand for nickel
and stainless fastener material increased year over year for the ninth
consecutive quarter ― while shipment of titanium fastener material set a
new first quarter record following a record fourth quarter. Sales of
Carpenter’s Custom-series stainless alloys and the addition of Latrobe’s
structural, bearing and other complementary products also contributed to
the year-to-year growth rate.
Energy market sales of $77.4 million increased 31 percent
compared to the same period a year ago. Excluding surcharge revenue,
energy market sales increased 38 percent on 20 percent higher volume (or
flat revenues on 6 percent higher volume without Latrobe). Contributing
to the overall sales growth is the inclusion this quarter of the
Specialty Steel Supply (SSS) distribution sales that do not have related
manufacturing volume. While North American rig activity has been
slowing, Carpenter has maintained growth in oil & gas through continued
share gain, an expanding geographic footprint, and increased
participation in other applications like completions. Market trends
supporting increased use of industrial gas turbines are expected to be a
future growth driver, despite the temporary slowness in project activity
in this area.
Medical market sales were $30.4 million in the first quarter,
down 8 percent from a year ago. Excluding surcharge revenue, medical
market sales decreased 5 percent on 13 percent lower volume (relatively
unchanged without Latrobe). In general, medical customers are focused on
cost containment which is impacting inventory-on-hand strategies. In
addition, uncertainty surrounding pending legislative impacts and
economic sentiment is affecting short term demand. These current demand
factors are expected to change by the end of the fiscal year, and the
long term positive demand trend for Carpenter medical market sales
remains unchanged.
Transportation market sales were $34.5 million, an increase of 10
percent from a year earlier. Excluding surcharge revenue, transportation
sales increased 19 percent on 4 percent higher volume (or up 16 percent
on 2 percent higher volume without Latrobe). Revenue growth in excess of
volume growth reflects Carpenter’s continued focus on high-end specialty
automotive applications required to meet increasing fuel efficiency
standards. Demand is growing for high value materials required in
turbo-charger, gasket and fuel system applications. In addition,
commodity stainless steel materials are being replaced by higher value
nickel based alloys for engine valve applications that support higher
operating temperatures.
Industrial & Consumer market sales were $113.9 million in the
first quarter, up 8 percent compared with the same period a year ago.
Excluding surcharge revenue, sales increased 18 percent on 14 percent
higher volume (or up 3 percent on 1 percent higher volume without
Latrobe). Although this market is more sensitive to economic
uncertainty, Carpenter’s strategy has been to focus on specialized, high
value niche applications with strategically important customers. This
strategy offsets softness in more commodity type products and
distributor channel sales.
International sales in the first quarter were $163.8 million, an
increase of 19 percent compared with the same quarter a year earlier -
driven by a 41 percent increase in Asia/Pacific sales and a 14 percent
increase in European sales. Growth in Asia/Pacific was led by sales into
the aerospace and energy end markets. In particular, there is a
significant increase in activity by Chinese aerospace forging customers
and the Japanese aerospace supply chain. Growth in Europe was led by
increased demand for materials used for aerospace and high value
automotive applications. Total international sales in the quarter
represented 30 percent of total Company revenue compared with 33 percent
in the prior year. Excluding Latrobe, total international sales in the
quarter represented 35 percent of sales compared with 33 percent in the
prior year.
Pension Effects
During the first quarter, the Company recorded expense associated with
its pension and other post retirement benefit plans of $17.2 million or
$0.21 per diluted share. Pension expense in the prior year first quarter
was $9.9 million or $0.14 per diluted share. The Company made cash
contributions of $48.1 million during the first quarter of fiscal year
2013, and expects to make additional minimum cash contributions of
approximately $34 million over the balance of fiscal year 2013. Due to
favorable credit market conditions and the impact that historically low
interest rates have had on pension funding requirements, the Company
continues to plan for a debt issuance in the third fiscal quarter that
would replace the May 2013 debt maturity and could provide the
opportunity to fund an additional discretionary pension contribution of
about $150 million. This would increase the funded status of the plans,
and reduce required cash contributions and non-cash pension expense over
the next several years.
Non-GAAP Financial Measures
This press release includes discussions of financial measures that have
not been determined in accordance with U.S. generally accepted
accounting principles ("GAAP"). The non-GAAP financial measures,
accompanied by reasons why the Company believes the measures are
important, are included in the attached schedules.
Conference Call
Carpenter will host a conference call and webcast today, October 23, at
10:00 a.m., ET, to discuss financial results and operations for the
fiscal first quarter. Please call 610-208-2222 for details of the
conference call. Access to the call will also be made available at
Carpenter's web site (http://www.cartech.com)
and through CCBN (http://www.ccbn.com).
A replay of the call will be made available at http://www.cartech.com
or at http://www.ccbn.com.
About Carpenter Technology
Carpenter produces and distributes premium alloys, including special
alloys, titanium alloys and powder metals, as well as stainless steels,
and alloy and tool steels. Information about Carpenter can be found on
the Internet at http://www.cartech.com.
Forward-Looking Statements
This press release contains forward-looking statements within the
meaning of the Private Securities Litigation Act of 1995. These
forward-looking statements are subject to risks and uncertainties that
could cause actual results to differ from those projected, anticipated
or implied. The most significant of these uncertainties are described in
Carpenter’s filings with the Securities and Exchange Commission
including its annual report on Form 10-K for the year ended June 30,
2012 and the exhibits attached to that filing. They include but are not
limited to: (1) expectations with respect to the synergies, costs and
other anticipated financial impacts of the Latrobe acquisition
transaction could differ from actual synergies realized, costs incurred
and financial impacts experienced as a result of the transaction; (2)
the cyclical nature of the specialty materials business and certain
end-use markets, including aerospace, defense, industrial,
transportation, consumer, medical, and energy, or other influences on
Carpenter’s business such as new competitors, the consolidation of
competitors, customers, and suppliers or the transfer of manufacturing
capacity from the United States to foreign countries;(3) the ability of
Carpenter to achieve cost savings, productivity improvements or process
changes; (4) the ability to recoup increases in the cost of energy, raw
materials, freight or other factors; (5) domestic and foreign excess
manufacturing capacity for certain metals; (6) fluctuations in currency
exchange rates; (7) the degree of success of government trade actions;
(8) the valuation of the assets and liabilities in Carpenter’s pension
trusts and the accounting for pension plans; (9) possible labor disputes
or work stoppages; (10) the potential that our customers may substitute
alternate materials or adopt different manufacturing practices that
replace or limit the suitability of our products; (11) the ability to
successfully acquire and integrate acquisitions, including the Latrobe
acquisition; (12) the availability of credit facilities to Carpenter,
its customers or other members of the supply chain; (13) the ability to
obtain energy or raw materials, especially from suppliers located in
countries that may be subject to unstable political or economic
conditions; (14) Carpenter’s manufacturing processes are dependent upon
highly specialized equipment located primarily in facilities in Reading
and Latrobe, Pennsylvania for which there may be limited alternatives if
there are significant equipment failures or catastrophic event; and (15)
Carpenter’s future success depends on the continued service and
availability of key personnel, including members of our executive
management team, management, metallurgists and other skilled personnel
and the loss of these key personnel could affect our ability to perform
until suitable replacements are found. Any of these factors could have
an adverse and/or fluctuating effect on Carpenter’s results of
operations. The forward-looking statements in this document are intended
to be subject to the safe harbor protection provided by Section 27A of
the Securities Act of 1933, as amended, and Section 21E of the
Securities Exchange Act of 1934, as amended. Carpenter undertakes no
obligation to update or revise any forward-looking statements.
|
|
|
PRELIMINARY
|
|
CONSOLIDATED BALANCE SHEETS
|
|
(in millions)
|
|
(Unaudited)
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
September 30,
|
|
June 30,
|
|
|
|
|
|
|
|
|
2012
|
|
2012
|
|
|
|
|
|
|
|
|
|
|
|
|
ASSETS
|
|
|
|
|
|
|
|
|
|
|
Current assets:
|
|
|
|
|
|
|
|
|
|
Cash and cash equivalents
|
|
|
|
|
$
|
112.6
|
|
|
$
|
211.0
|
|
|
Accounts receivable, net
|
|
|
|
|
|
319.5
|
|
|
|
354.2
|
|
|
Inventories
|
|
|
|
|
|
|
722.2
|
|
|
|
642.0
|
|
|
Deferred income taxes
|
|
|
|
|
|
-
|
|
|
|
10.6
|
|
|
Other current assets
|
|
|
|
|
|
|
37.6
|
|
|
|
31.9
|
|
|
Total current assets
|
|
|
|
|
|
1,191.9
|
|
|
|
1,249.7
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Property, plant and equipment, net
|
|
|
|
|
959.7
|
|
|
|
924.6
|
|
|
Goodwill
|
|
|
|
|
|
|
|
261.2
|
|
|
|
260.5
|
|
|
Other intangibles, net
|
|
|
|
|
|
|
106.5
|
|
|
|
109.9
|
|
|
Other assets
|
|
|
|
|
|
|
83.8
|
|
|
|
83.1
|
|
|
Total assets
|
|
|
|
|
|
$
|
2,603.1
|
|
|
$
|
2,627.8
|
|
|
|
|
|
|
|
|
|
|
|
|
|
LIABILITIES
|
|
|
|
|
|
|
|
|
|
Current liabilities:
|
|
|
|
|
|
|
|
|
|
Accounts payable
|
|
|
|
|
|
$
|
235.8
|
|
|
$
|
236.1
|
|
|
Accrued liabilities
|
|
|
|
|
|
|
179.6
|
|
|
|
217.1
|
|
|
Deferred income taxes
|
|
|
|
|
|
2.5
|
|
|
|
-
|
|
|
Current portion of long-term debt
|
|
|
|
|
101.0
|
|
|
|
101.0
|
|
|
Total current liabilities
|
|
|
|
|
|
518.9
|
|
|
|
554.2
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Long-term debt, net of current portion
|
|
|
|
|
305.6
|
|
|
|
305.9
|
|
|
Accrued pension liabilities
|
|
|
|
|
|
340.1
|
|
|
|
377.3
|
|
|
Accrued postretirement benefits
|
|
|
|
|
|
178.7
|
|
|
|
179.8
|
|
|
Deferred income taxes
|
|
|
|
|
|
32.2
|
|
|
|
31.4
|
|
|
Other liabilities
|
|
|
|
|
|
|
52.2
|
|
|
|
66.1
|
|
|
Total liabilities
|
|
|
|
|
|
|
1,427.7
|
|
|
|
1,514.7
|
|
|
|
|
|
|
|
|
|
|
|
|
|
STOCKHOLDERS' EQUITY
|
|
|
|
|
|
|
|
|
Carpenter stockholders' equity:
|
|
|
|
|
|
|
|
|
Common stock
|
|
|
|
|
|
|
274.3
|
|
|
|
274.0
|
|
|
Capital in excess of par value
|
|
|
|
|
|
247.9
|
|
|
|
252.7
|
|
|
Reinvested earnings
|
|
|
|
|
|
|
1,139.2
|
|
|
|
1,109.6
|
|
|
Common stock in treasury, at cost
|
|
|
|
|
(111.7
|
)
|
|
|
(120.0
|
)
|
|
Accumulated other comprehensive loss
|
|
|
|
|
(384.1
|
)
|
|
|
(412.5
|
)
|
|
Total Carpenter stockholders' equity
|
|
|
|
|
1,165.6
|
|
|
|
1,103.8
|
|
|
Noncontrolling interest
|
|
|
|
|
|
9.8
|
|
|
|
9.3
|
|
|
Total equity
|
|
|
|
|
|
|
1,175.4
|
|
|
|
1,113.1
|
|
|
Total liabilities and equity
|
|
|
|
|
$
|
2,603.1
|
|
|
$
|
2,627.8
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
PRELIMINARY
|
|
CONSOLIDATED STATEMENTS OF INCOME
|
|
(in millions, except per share data)
|
|
(Unaudited)
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Three Months Ended
|
|
|
|
|
|
|
September 30,
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
2012
|
|
2011
|
|
|
|
|
|
|
|
|
|
|
NET SALES
|
|
|
|
$
|
544.9
|
|
|
$
|
414.1
|
|
|
Cost of sales
|
|
|
|
|
435.6
|
|
|
|
333.0
|
|
|
Gross profit
|
|
|
|
|
109.3
|
|
|
|
81.1
|
|
|
|
|
|
|
|
|
|
|
|
Selling, general and administrative expenses
|
|
|
47.7
|
|
|
|
35.7
|
|
|
Acquisition-related costs
|
|
|
|
-
|
|
|
|
1.4
|
|
|
Operating income
|
|
|
|
|
61.6
|
|
|
|
44.0
|
|
|
|
|
|
|
|
|
|
|
|
Interest expense
|
|
|
|
|
(5.2
|
)
|
|
|
(7.0
|
)
|
|
Other income (expense), net
|
|
|
|
2.7
|
|
|
|
(0.7
|
)
|
|
|
|
|
|
|
|
|
|
|
Income before income taxes
|
|
|
|
59.1
|
|
|
|
36.3
|
|
|
Income tax expense
|
|
|
|
|
19.6
|
|
|
|
12.6
|
|
|
|
|
|
|
|
|
|
|
|
Net income
|
|
|
|
|
39.5
|
|
|
|
23.7
|
|
|
|
|
|
|
|
|
|
|
|
Less: Net income (loss) attributable to noncontrolling interest
|
|
|
0.3
|
|
|
|
(0.1
|
)
|
|
|
|
|
|
|
|
|
|
|
NET INCOME ATTRIBUTABLE TO CARPENTER
|
|
$
|
39.2
|
|
|
$
|
23.8
|
|
|
|
|
|
|
|
|
|
|
|
EARNINGS PER SHARE:
|
|
|
|
|
|
|
Basic
|
|
|
|
|
$
|
0.74
|
|
|
$
|
0.53
|
|
|
Diluted
|
|
|
|
|
$
|
0.74
|
|
|
$
|
0.53
|
|
|
|
|
|
|
|
|
|
|
|
WEIGHTED AVERAGE SHARES
|
|
|
|
|
|
OUTSTANDING:
|
|
|
|
|
|
|
|
Basic
|
|
|
|
|
|
52.8
|
|
|
|
44.3
|
|
|
Diluted
|
|
|
|
|
|
53.4
|
|
|
|
45.1
|
|
|
|
|
|
|
|
|
|
|
|
Cash dividends per common share
|
|
$
|
0.18
|
|
|
$
|
0.18
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
PRELIMINARY
|
|
CONSOLIDATED STATEMENTS OF CASH FLOWS
|
|
(in millions)
|
|
(Unaudited)
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Three Months Ended
|
|
|
|
|
|
|
|
|
September 30,
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
2012
|
|
2011
|
|
|
|
|
|
|
|
|
|
|
|
|
OPERATING ACTIVITIES:
|
|
|
|
|
|
|
|
|
Net income
|
|
|
|
|
|
$
|
39.5
|
|
|
$
|
23.7
|
|
|
Adjustments to reconcile net income to net cash
|
|
|
|
|
|
|
used for operating activities:
|
|
|
|
|
|
|
|
|
Depreciation and amortization
|
|
|
|
|
|
25.5
|
|
|
|
18.5
|
|
|
Deferred income taxes
|
|
|
|
|
|
0.1
|
|
|
|
6.1
|
|
|
Net pension expense
|
|
|
|
|
|
17.2
|
|
|
|
9.9
|
|
|
Net loss on disposal of property and equipment
|
|
|
|
0.1
|
|
|
|
-
|
|
|
Changes in working capital and other:
|
|
|
|
|
|
|
|
Accounts receivable
|
|
|
|
|
|
36.1
|
|
|
|
0.8
|
|
|
Inventories
|
|
|
|
|
|
|
(78.7
|
)
|
|
|
(94.9
|
)
|
|
Other current assets
|
|
|
|
|
|
(4.7
|
)
|
|
|
(1.6
|
)
|
|
Accounts payable
|
|
|
|
|
|
|
(0.5
|
)
|
|
|
9.3
|
|
|
Accrued liabilities
|
|
|
|
|
|
|
(23.5
|
)
|
|
|
(13.4
|
)
|
|
Pension contribution
|
|
|
|
|
|
(48.1
|
)
|
|
|
(11.6
|
)
|
|
Boarhead Farms settlement
|
|
|
|
|
|
-
|
|
|
|
(21.8
|
)
|
|
Other, net
|
|
|
|
|
|
|
0.3
|
|
|
|
1.0
|
|
|
Net cash used for operating activities
|
|
|
|
|
(36.7
|
)
|
|
|
(74.0
|
)
|
|
|
|
|
|
|
|
|
|
|
|
|
INVESTING ACTIVITIES:
|
|
|
|
|
|
|
|
|
Purchases of property, equipment and software
|
|
|
|
(56.4
|
)
|
|
|
(27.3
|
)
|
|
Proceeds from disposals of property and equipment
|
|
|
|
-
|
|
|
|
0.2
|
|
|
Proceeds from sales and maturities of marketable securities
|
|
|
-
|
|
|
|
30.4
|
|
|
Net cash (used for) provided from investing activities
|
|
|
|
(56.4
|
)
|
|
|
3.3
|
|
|
|
|
|
|
|
|
|
|
|
|
|
FINANCING ACTIVITIES:
|
|
|
|
|
|
|
|
|
Payments on long-term debt
|
|
|
|
|
|
-
|
|
|
|
(100.0
|
)
|
|
Dividends paid
|
|
|
|
|
|
|
(9.6
|
)
|
|
|
(8.1
|
)
|
|
Tax benefits on share-based compensation
|
|
|
|
3.0
|
|
|
|
0.6
|
|
|
Proceeds from stock options exercised
|
|
|
|
|
1.1
|
|
|
|
0.7
|
|
|
Net cash used for financing activities
|
|
|
|
|
(5.5
|
)
|
|
|
(106.8
|
)
|
|
|
|
|
|
|
|
|
|
|
|
|
Effect of exchange rate changes on cash and cash equivalents
|
|
|
0.2
|
|
|
|
(0.2
|
)
|
|
|
|
|
|
|
|
|
|
|
|
|
DECREASE IN CASH AND CASH EQUIVALENTS
|
|
|
(98.4
|
)
|
|
|
(177.7
|
)
|
|
Cash and cash equivalents at beginning of period
|
|
|
|
211.0
|
|
|
|
492.5
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Cash and cash equivalents at end of period
|
|
|
|
|
112.6
|
|
|
|
314.8
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
PRELIMINARY
|
|
SEGMENT FINANCIAL DATA
|
|
(in millions, except pounds sold)
|
|
(Unaudited)
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Three Months Ended
|
|
|
|
|
|
|
September 30,
|
|
|
|
|
|
|
2012
|
|
2011
|
|
Pounds sold* (000):
|
|
|
|
|
|
Specialty Alloys Operations
|
|
|
47,212
|
|
|
|
44,210
|
|
|
Performance Engineered Products
|
|
|
3,384
|
|
|
|
3,438
|
|
|
Latrobe
|
|
|
|
16,108
|
|
|
|
-
|
|
|
Intersegment
|
|
|
(2,690
|
)
|
|
|
(620
|
)
|
|
|
|
|
|
|
|
|
|
|
Consolidated pounds sold
|
|
|
64,014
|
|
|
|
47,028
|
|
|
|
|
|
|
|
|
|
|
|
Net sales:
|
|
|
|
|
|
|
Specialty Alloys Operations
|
|
|
|
|
|
|
Net sales excluding surcharge
|
|
$
|
272.9
|
|
|
$
|
234.5
|
|
|
|
Surcharge
|
|
|
88.9
|
|
|
|
101.3
|
|
|
|
|
|
|
|
|
|
|
|
Specialty Alloys Operations net sales
|
|
|
361.8
|
|
|
|
335.8
|
|
|
|
|
|
|
|
|
|
|
|
Performance Engineered Products
|
|
|
|
|
|
|
Net sales excluding surcharge
|
|
|
97.6
|
|
|
|
83.0
|
|
|
|
Surcharge
|
|
|
1.1
|
|
|
|
1.2
|
|
|
|
|
|
|
|
|
|
|
|
Performance Engineered Products net sales
|
|
|
98.7
|
|
|
|
84.2
|
|
|
|
|
|
|
|
|
|
|
|
Latrobe
|
|
|
|
|
|
|
|
Net sales excluding surcharge
|
|
|
106.2
|
|
|
|
10.2
|
|
|
|
Surcharge
|
|
|
15.6
|
|
|
|
-
|
|
|
|
|
|
|
|
|
|
|
|
Latrobe net sales
|
|
|
121.8
|
|
|
|
10.2
|
|
|
|
|
|
|
|
|
|
|
|
Intersegment
|
|
|
|
|
|
|
Net sales excluding surcharge
|
|
|
(35.9
|
)
|
|
|
(14.1
|
)
|
|
|
Surcharge
|
|
|
(1.5
|
)
|
|
|
(2.0
|
)
|
|
Intersegment net sales
|
|
|
(37.4
|
)
|
|
|
(16.1
|
)
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Consolidated net sales
|
|
$
|
544.9
|
|
|
$
|
414.1
|
|
|
|
|
|
|
|
|
|
|
|
Operating income:
|
|
|
|
|
|
Specialty Alloys Operations
|
|
$
|
54.4
|
|
|
$
|
46.3
|
|
|
Performance Engineered Products
|
|
|
11.5
|
|
|
|
11.8
|
|
|
Latrobe
|
|
|
|
15.7
|
|
|
|
0.6
|
|
|
Corporate costs (including acquisition-related costs)
|
|
|
(10.4
|
)
|
|
|
(10.2
|
)
|
|
Pension earnings, interest & deferrals
|
|
|
(8.0
|
)
|
|
|
(3.6
|
)
|
|
Intersegment
|
|
|
(1.6
|
)
|
|
|
(0.9
|
)
|
|
|
|
|
|
|
|
|
|
|
Consolidated operating income
|
|
$
|
61.6
|
|
|
$
|
44.0
|
|
|
|
|
|
|
|
|
|
|
|
|
In January 2012, the Company announced it had made changes to its
reportable segments. The Company now has three reportable business
segments, Specialty Alloys Operations (SAO), Performance Engineered
Products (PEP) and Latrobe. Previously, the Company's reportable
segments consisted of Premium Alloys Operations (PAO), Advanced
Metals Operations (AMO) and Emerging Ventures.
|
|
|
|
|
The SAO segment is comprised of Carpenter's major premium alloy and
stainless steel manufacturing operations. This includes operations
performed at mills primarily in Reading, Pennsylvania and the
surrounding area, South Carolina, and the new premium products
manufacturing facility being built in Limestone County, Alabama.
|
|
|
|
|
The Latrobe segment is comprised of the operations of the Latrobe
business acquired effective February 29, 2012. The Latrobe segment
provides management with the focus and visibility into the business
performance of these newly acquired operations. The Latrobe segment
also includes the results of Carpenter’s distribution business in
Mexico, which is being managed together with the Latrobe's
distribution business. As the Latrobe business becomes integrated
with Carpenter, its results will likely be reported within the SAO
business segment sometime in the future.
|
|
|
|
|
The service cost component of net pension expense, which represents
the estimated cost of future pension liabilities earned associated
with active employees, is included in the operating results of the
business segments. The residual net pension expense, or pension
earning, interest and deferrals (pension EID), is comprised of the
expected return on plan assets, interest costs on the projected
benefit obligations of the plans, and amortization of actuarial
gains and losses and prior service costs, is included under the
heading "Pension earnings, interest & deferrals."
|
|
|
|
|
* Pounds sold excludes sales associated with the distribution
businesses.
|
|
PRELIMINARY
|
|
NON-GAAP FINANCIAL MEASURES
|
|
(in millions, except per share data)
|
|
(Unaudited)
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Three Months Ended
|
|
|
|
|
|
|
September 30,
|
|
FREE CASH FLOW
|
|
|
2012
|
|
2011
|
|
Net cash used for operating activities
|
|
$
|
(36.7
|
)
|
|
$
|
(74.0
|
)
|
|
Purchases of property, equipment and software
|
|
|
(56.4
|
)
|
|
|
(27.3
|
)
|
|
Proceeds from disposals of property and equipment
|
|
|
-
|
|
|
|
0.2
|
|
|
Dividends paid
|
|
|
|
|
(9.6
|
)
|
|
|
(8.1
|
)
|
|
|
|
|
|
|
|
|
|
|
Free cash flow
|
|
|
|
$
|
(102.7
|
)
|
|
$
|
(109.2
|
)
|
|
Management believes that the free cash flow measure provides useful
information to investors regarding our financial condition because
it is a measure of cash generated which management evaluates for
alternative uses.
|
|
|
|
|
|
|
Three Months Ended
|
|
|
|
|
|
|
September 30,
|
|
NET PENSION EXPENSE PER DILUTED SHARE
|
|
2012
|
|
2011
|
|
|
|
|
|
|
|
|
|
|
Pension plans expense
|
|
|
$
|
14.9
|
|
|
$
|
9.5
|
|
|
Other postretirement benefits expense
|
|
|
2.3
|
|
|
|
0.4
|
|
|
Net pension expense
|
|
|
|
17.2
|
|
|
|
9.9
|
|
|
Income tax benefit
|
|
|
|
(6.0
|
)
|
|
|
(3.8
|
)
|
|
Net pension expense, net of tax
|
|
$
|
11.2
|
|
|
$
|
6.1
|
|
|
|
|
|
|
|
|
|
|
|
Net pension expense per diluted share
|
|
$
|
0.21
|
|
|
$
|
0.14
|
|
|
|
|
|
|
|
|
|
|
|
Weighted average diluted common shares
|
|
|
53.4
|
|
|
|
45.1
|
|
|
Management believes that net pension expense per diluted share is
helpful in analyzing the operating performance of the Company, as
net pension expense may be volatile due to changes in the financial
markets, which may result in significant fluctuations in operating
results from period to period.
|
|
OPERATING MARGIN EXCLUDING SURCHARGE AND
|
|
Three Months Ended
|
|
PENSION EARNINGS, INTEREST AND DEFERRALS
|
|
September 30,
|
|
|
|
|
|
|
2012
|
|
2011
|
|
|
|
|
|
|
|
|
|
|
Net sales
|
|
|
|
$
|
544.9
|
|
|
$
|
414.1
|
|
|
Less: surcharge revenue
|
|
|
|
104.1
|
|
|
|
100.5
|
|
|
Consolidated net sales excluding surcharge
|
|
$
|
440.8
|
|
|
$
|
313.6
|
|
|
|
|
|
|
|
|
|
|
|
Operating income
|
|
|
|
$
|
61.6
|
|
|
$
|
44.0
|
|
|
Pension earnings, interest & deferrals
|
|
|
8.0
|
|
|
|
3.6
|
|
|
Operating income excluding pension earnings, interest
|
|
|
|
|
|
and deferrals
|
|
|
|
$
|
69.6
|
|
|
$
|
47.6
|
|
|
|
|
|
|
|
|
|
|
|
Operating margin excluding surcharge and pension earnings, interest
|
|
|
|
|
|
and deferrals
|
|
|
|
|
15.8
|
%
|
|
|
15.2
|
%
|
|
Management believes that removing the impacts of raw material
surcharges from operating margin provides a more consistent basis
for comparing results of operations from period to period. In
addition, management believes that excluding the impact of pension
earnings, interest and deferrals, which may be volatile due to
changes in the financial markets, is helpful in analyzing the true
operating performance of the Company.
|
|
PRELIMINARY
|
|
NON-GAAP FINANCIAL MEASURES
|
|
(in millions, except per share data)
|
|
(Unaudited)
|
|
|
|
|
|
|
|
|
|
Three Months Ended
September 30,
|
|
ADJUSTED LATROBE OPERATING RESULTS
|
|
2012
|
|
2011
|
|
|
|
|
|
|
|
Latrobe segment operating income
|
|
$
|
15.7
|
|
|
$
|
0.6
|
|
|
Specialty Steel Supply operating income included in Performance
Engineered Products segment results
|
|
|
1.9
|
|
|
|
-
|
|
|
Carpenter distribution business operating income in Mexico included in
Latrobe segment results
|
|
|
(0.7
|
)
|
|
|
(0.6
|
)
|
|
Latrobe pension EID included in pension EID expense
|
|
|
(0.6
|
)
|
|
|
-
|
|
|
Adjusted Latrobe operating results before income taxes
|
|
|
16.3
|
|
|
|
-
|
|
|
Income taxes
|
|
|
(5.7
|
)
|
|
|
-
|
|
|
Adjusted Latrobe operating results
|
|
$
|
10.6
|
|
|
$
|
-
|
|
|
|
|
|
|
|
|
Adjusted Latrobe operating results per diluted share
|
|
$
|
0.20
|
|
|
$
|
-
|
|
|
Dilutive impact of shares issued in connection with Latrobe
acquisition*
|
|
|
(0.13
|
)
|
|
|
-
|
|
|
|
|
|
|
|
|
Net accretion from Latrobe's operating results
|
|
$
|
0.07
|
|
|
$
|
-
|
|
|
|
|
|
|
|
|
Weighted average shares outstanding
|
|
|
53.4
|
|
|
|
45.1
|
|
|
* In connection with the Latrobe Acquisition, Carpenter issued
shares of common stock to the former
owners which resulted in an additional 8.1 million weighted
average shares during the three months ended
September 30, 2012.
|
|
IMPACTS OF FACILITY START-UP, MANUFACTURING FOOTPRINT OPTIMIZATION
AND INVENTORY REDUCTION INITIATIVE COSTS
|
|
Three Months Ended
September 30,
|
|
|
|
2012
|
|
2011
|
|
|
|
|
|
|
|
Facility start-up costs
|
|
$
|
0.9
|
|
|
$
|
-
|
|
|
Manufacturing footprint optimization costs
|
|
|
0.1
|
|
|
|
-
|
|
|
Inventory reduction initiative costs
|
|
|
0.6
|
|
|
|
-
|
|
|
Operating income impact
|
|
$
|
1.6
|
|
|
$
|
-
|
|
|
|
|
|
|
|
|
Consolidated net sales excluding surcharges
|
|
$
|
440.8
|
|
|
$
|
313.6
|
|
|
|
|
|
|
|
|
Impact of facility start-up, manufacturing footprint optimization
and inventory
reduction initiative costs on operating margin excluding surcharges
|
|
|
0.4
|
%
|
|
|
0.0
|
%
|
|
|
|
|
|
|
|
Operating income impact
|
|
$
|
1.6
|
|
|
$
|
-
|
|
|
Income tax benefit
|
|
|
(0.6
|
)
|
|
|
-
|
|
|
Net income impact
|
|
$
|
1.0
|
|
|
$
|
-
|
|
|
|
|
|
|
|
|
Impact per diluted share
|
|
$
|
0.02
|
|
|
$
|
-
|
|
|
|
|
|
|
|
|
Weighted average shares outstanding
|
|
|
53.4
|
|
|
|
45.1
|
|
|
Management believes that removing the impacts of costs associated
with (i.) start-up of our Athens, AL facility, (ii.) manufacturing
footprint optimization associated with evaluating and executing
opportunities primarily as a result of the Latrobe acquisition to
optimize manufacturing efficiencies, and (iii.) an inventory
reduction initiative aimed at identifying opportunities reduce
inventory levels and improve inventory turnover across the mill
operations are helpful in analyzing the operating performance of the
Company, as these costs are expected to be nonrecurring in nature
and may result in significant fluctuations in operating results from
period to period during fiscal years 2013 and 2014.
|
|
PRELIMINARY
|
|
SUPPLEMENTAL SCHEDULES
|
|
(in millions)
|
|
(Unaudited)
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Three Months Ended
|
|
|
|
|
|
|
September 30,
|
|
NET SALES BY END USE MARKET
|
|
2012
|
|
2011
|
|
|
|
|
|
|
|
|
|
|
End Use Market Excluding Surcharge:
|
|
|
|
|
|
Aerospace and defense
|
|
|
$
|
195.3
|
|
$
|
128.3
|
|
Industrial and consumer
|
|
|
|
86.6
|
|
|
73.5
|
|
Energy
|
|
|
|
|
|
69.4
|
|
|
50.4
|
|
Transportation
|
|
|
|
|
26.1
|
|
|
22.0
|
|
Medical
|
|
|
|
|
|
27.8
|
|
|
29.2
|
|
Distribution
|
|
|
|
|
35.6
|
|
|
10.2
|
|
|
|
|
|
|
|
|
|
|
Consolidated net sales excluding surcharge
|
|
|
440.8
|
|
|
313.6
|
|
|
|
|
|
|
|
|
|
|
Surcharge revenue
|
|
|
|
|
104.1
|
|
|
100.5
|
|
|
|
|
|
|
|
|
|
|
Consolidated net sales
|
|
|
$
|
544.9
|
|
$
|
414.1
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Three Months Ended
|
|
|
|
|
|
|
September 30,
|
|
NET SALES BY MAJOR PRODUCT CLASS
|
|
2012
|
|
2011
|
|
|
|
|
|
|
|
|
|
|
Net Sales by Product Class Excluding Surcharge:
|
|
|
|
|
|
Special alloys
|
|
|
|
$
|
168.9
|
|
$
|
128.0
|
|
Stainless steel
|
|
|
|
|
120.9
|
|
|
111.9
|
|
Titanium products
|
|
|
|
|
39.7
|
|
|
38.6
|
|
Powder metals
|
|
|
|
|
14.8
|
|
|
13.8
|
|
Alloy and tool steel
|
|
|
|
54.0
|
|
|
5.2
|
|
Distribution and other
|
|
|
|
42.5
|
|
|
16.1
|
|
|
|
|
|
|
|
|
|
|
Consolidated net sales excluding surcharge
|
|
|
440.8
|
|
|
313.6
|
|
|
|
|
|
|
|
|
|
|
Surcharge revenue
|
|
|
|
|
104.1
|
|
|
100.5
|
|
|
|
|
|
|
|
|
|
|
Consolidated net sales
|
|
|
$
|
544.9
|
|
$
|
414.1
|
Source: Carpenter Technology Corporation
Carpenter Technology Corporation
Media Inquiries:
William J.
Rudolph, Jr., 610-208-3892
wrudolph@cartech.com
or
Investor
Inquiries:
Michael A. Hajost, 610-208-3476
mhajost@cartech.com